Portland cement 42.5N
Russian Standard GOST 10178-85, 30515-97
Class of strength (type): portland cement 400 (42.5N)
Mineral additives: 28.6 %
Normal thickness of the cement test: 26.2
Average activity with the steaming: 30.5 MPa
Value of the specific effectiveness of the activity of the natural radionuclides: 59.7 Bq/kg, with the standard level no more than 60 Bq/kg.
|
The chemical composition of cement (%)
- Content of the oxide of magnesium MgO in clinker 2.50
- Content of the oxide of sulfur (THE VI) SO3 2.46
- Content of chlorion Cl- 0.002
- Mass fraction of the alkaline oxides R2O 0,62
Mineralogical composition of clinker (%)
- Ca3Si (tricalcium silicate) 68.69
- Ca2Si (dicalcium silicate) 11.14
- Ca3Al (tricalcium aluminate) 9.20
- Ca4AlFe (dicalcium alumo-ferrite) 10.69
|
|